SM 1.6 mm Round + GW 90 mm R2.5 + MLV
Sheet Metal 1.6 mm Round · Glass Wool 90 mm R2.5 · MLV
Tested 16 July 2026
Rw (C; Ctr)
29dB
C −2 · Ctr −5
ΔRw vs open
+28dB
Fit to R − R(open aperture)
Mean R
25.5dB
100–3150 Hz
Rank by Rw
7of 64
Tied with 3 others
Specification
Panel
- Panel
- Sheet Metal 1.6 mm Round
- Perforation
- Round, Ø1.6 mm
- Open area
- 23.0 %
- Panel thickness
- 1.2 mm
- Scrim
- No
- Orientation
- Standard
Insulation
- Insulation
- Glass wool
- Thickness
- 90 mm
- Thermal R-value
- R2.5
- Flow resistivity σ
- 17.1k N·s/m⁴measured 14.4k–21.4k
- Flow resistance σ·d
- 1.5k N·s/m³
Mass-loaded vinyl
- MLV
- Yes, 4 kg nominal
Test
- Tested
- 16 July 2026
- Matrix group
- MLV
Band values
| Hz | R | Ref. | Dev. | T60 | αs |
|---|---|---|---|---|---|
| 50 | – | – | – | ||
| 63 | 13.8 | 14.18 | – | ||
| 80 | 12.1 | 9.10 | – | ||
| 100 | 16.9 | 10 | 0.0 | 7.64 | 0.02 |
| 125 | 16.4 | 13 | 0.0 | 6.60 | 0.52 |
| 160 | 14.1 | 16 | 1.9 | 7.27 | 0.44 |
| 200 | 13.6 | 19 | 5.4 | 6.11 | 0.22 |
| 250 | 16.6 | 22 | 5.4 | 5.58 | 0.22 |
| 315 | 19.6 | 25 | 5.4 | 5.29 | 0.25 |
| 400 | 22.1 | 28 | 5.9 | 5.01 | 0.01 |
| 500 | 25.4 | 29 | 3.6 | 5.47 | 0.10 |
| 630 | 28.4 | 30 | 1.6 | 5.38 | 0.17 |
| 800 | 31.4 | 31 | 0.0 | 5.29 | 0.18 |
| 1k | 32.8 | 32 | 0.0 | 4.66 | 0.20 |
| 1.25k | 32.4 | 33 | 0.6 | 4.16 | 0.25 |
| 1.6k | 31.4 | 33 | 1.6 | 3.84 | 0.29 |
| 2k | 34.4 | 33 | 0.0 | 3.40 | 0.54 |
| 2.5k | 36.5 | 33 | 0.0 | 3.10 | 0.53 |
| 3.15k | 36.5 | 33 | 0.0 | 2.73 | 0.75 |
| 4k | 41.8 | 2.32 | 1.08 | ||
| 5k | 44.5 | 1.81 | 1.73 | ||
| 6.3k | 50.3 | 1.43 | – | ||
| 8k | 52.0 | 1.12 | – | ||
| 10k | 54.0 | 0.92 | – | ||
| Σ | 31.6 |
R, Ref. and Dev. in dB, T60 in s. Ref. is the ISO 717-1 reference curve shifted to Rw 29 dB; Dev. is how far R falls below it, and the deviations may total at most 32 dB. αs over 100 Hz–5 kHz only.
In comparisons3
Sets of tests that differ from this one in a single variable.