Tests
6
first: No Insulation
Rw range
7–25dB
spread 18 dB
Highest Rw
25dB
GW 210 mm R5 (23,300 N·s/m⁴)
Largest ΔRw vs first
+17dB
GW 210 mm R5 (23,300 N·s/m⁴)
Sound reduction index (R)
R′ from the B&K 2270, re-referenced to the 0.9216 m² specimen area (−0.35 dB; −10.96 dB for the 22 Sep tests, logged with S = 11.5 m²). Grey lines: the open aperture (the opening with nothing in it) and unperforated 10 mm plasterboard.
Single-number ratings
Open in explorer- No InsulationC 0 · Ctr 0 · vs open +7 · mean R 8.37 dBfirst
- GW 100 mm R5 (9,600 N·s/m⁴)C −1 · Ctr −2 · vs open +16 · mean R 14.717 dB+9
- GW 175 mm R3.5 (10,200 N·s/m⁴)C 0 · Ctr −2 · vs open +19 · mean R 16.819 dB+12
- GW 45 mm R2.5 (14,800 N·s/m⁴)C 0 · Ctr −1 · vs open +14 · mean R 13.014 dB+7
- GW 90 mm R2.5 (17,100 N·s/m⁴)C 0 · Ctr −2 · vs open +19 · mean R 17.419 dB+12
- GW 210 mm R5 (23,300 N·s/m⁴)C −1 · Ctr −4 · vs open +24 · mean R 22.625 dB+17
| Listen | Varies | Rw | C | Ctr | ΔRw vs first | ΔRw vs open | Mean R | |
|---|---|---|---|---|---|---|---|---|
| No Insulation | 7 | 0 | 0 | ref. | +7 | 8.3 | ||
| GW 100 mm R5 (9,600 N·s/m⁴) | 17 | −1 | −2 | +9 | +16 | 14.7 | ||
| GW 175 mm R3.5 (10,200 N·s/m⁴) | 19 | 0 | −2 | +12 | +19 | 16.8 | ||
| GW 45 mm R2.5 (14,800 N·s/m⁴) | 14 | 0 | −1 | +7 | +14 | 13.0 | ||
| GW 90 mm R2.5 (17,100 N·s/m⁴) | 19 | 0 | −2 | +12 | +19 | 17.4 | ||
| GW 210 mm R5 (23,300 N·s/m⁴) | 25 | −1 | −4 | +17 | +24 | 22.6 |
Right: Rw, and below it ΔRw against the first test. Rw, C and Ctr per ISO 717-1 over 100–3150 Hz. ΔRw fits the reference curve to R − R(open aperture); ΔRw vs first is the difference between a test's ΔRw and the first test's, as the report quotes changes, so it can differ by a decibel from the change in Rw. Mean R is the arithmetic mean over the 16 rating bands.