Perforated Panel Acoustics

Effect of flow resistivity

Plasterboard 15 mm Round, No MLV

Insulation comparisons keyed on measured airflow resistivity.

Tests

5

first: No Insulation

Rw range

7–23dB

spread 16 dB

Highest Rw

23dB

GW 90 mm R2.7 (26,400 N·s/m⁴)

Largest ΔRw vs first

+16dB

GW 90 mm R2.7 (26,400 N·s/m⁴)

Sound reduction index (R)

R′ from the B&K 2270, re-referenced to the 0.9216 m² specimen area (−0.35 dB; −10.96 dB for the 22 Sep tests, logged with S = 11.5 m²). Grey lines: the open aperture (the opening with nothing in it) and unperforated 10 mm plasterboard.

Single-number ratings

Open in explorer
ListenVariesRwCCtrΔRw vs firstΔRw vs openMean R
No Insulation
7
00ref.+77.4
GW 100 mm R5 (9,600 N·s/m⁴)
16
−1−2+8+1513.8
GW 45 mm R2.5 (14,800 N·s/m⁴)
13
0−1+6+1312.0
GW 90 mm R2.5 (17,100 N·s/m⁴)
19
−1−3+11+1816.6
GW 90 mm R2.7 (26,400 N·s/m⁴)
23
0−3+16+2322.2

Right: Rw, and below it ΔRw against the first test. Rw, C and Ctr per ISO 717-1 over 100–3150 Hz. ΔRw fits the reference curve to R − R(open aperture); ΔRw vs first is the difference between a test's ΔRw and the first test's, as the report quotes changes, so it can differ by a decibel from the change in Rw. Mean R is the arithmetic mean over the 16 rating bands.